Paver Types
|
Paver Winter Durability Comparison |
| |
|
 Concrete Pavers
|
Concrete Pavers
High
Small, high density units resist cracking as well as damage from freeze-thaw and salts. Pavers are stronger than ordinary or stamped concrete.
|
 Cobble Stone
|
Cobble Stone
High
High density stone resists cracking and salts.
|
 Stamped Concrete
|
Stamped Concrete
Low
Subject to deterioration from de-icing salts. Surface sealer may provide some protection from salt attack.
|
 Clay Paver
|
Clay Paver
Moderate
Salts can attack and deteriorate some clay pavers.
|
 Ordinary Concrete
|
Ordinary Concrete
Low
Cracks from freeze-thaw, settlement and deteriorates from salts.
|
 Asphalt
|
Asphalt
Low
Cracks from freeze-thaw, settlement and deteriorates from de-icing salts.
|
 Crushed Stone or Gravel
|
Crushed Stone or Gravel
High
Stones resist freeze-thaw cycles and salts.
|